The modification of wetting properties in an electric field (electrowetting) is used for innovative technologies such as liquid lenses and special displays. The set PA3250 makes it possible to measure the contact angle with a voltage applied. This is achieved by voltage limiters (250 V) for DC and AC, insulators for the sample table and dosing unit, and connecting cables with crocodile clips. This makes it easy for you to use your intended voltage source for electrowetting analyses.