Product group specifications

Dosing System

Syringe Dosing

1 × single direct dosing

Drop deposition (syringe dosing)

software-controlled

Syringes, volume

disposable cartridge (1 mL)

Resolution (syringe dosing)

0.25 μL

Speed (syringe dosing)

2.7 µL/s – 100 µL/s

Camera system (standard)

Connection

USB 3.0

Performance

25 fps at 1000 × 700 px

Optics (standard)

Focus

fixed focus

Zoom

fixed focal length

View angle

2°

Field of view

4.7 mm × 3.3 mm

Resolution of optics

5 μm

Illumination

Types

high power LED

Wave length, dominant

468 nm

Field of light

5 mm × 23 mm (D × H)

Measurement specifications

Software

Software type

ADVANCE

Software languages

Chinese (simplified), English, French, German, Japanese, Korean, Portuguese, Russian, Spanish

Software modules

Contact angle (recommended)

Surface free energy of solids (optional)

Adhesion Analysis (optional)

Remote Control API (optional)

Sessile drop

Results

contact angle

Range

0 to 180° (software-based)

Resolution

0.01° (software-based)

Accuracy

0.8° (instrument-based)

Models

conic section
polynomial
circle
Young-Laplace
height-width

Types

static

Surface free energy of solids

Results

surface free energy
polar & disperse part
acid & base part
H-bond part

Models

equation of state
Zisman
Fowkes
Wu
Owens-Wendt-Rabel-Kaelble
extended Fowkes
acid-base theory

Constrained Sessile Drop

Results

surface tension

Range

0.01 to 2000 mN/m (software-based)

Resolution

0.01 mN/m (software-based)

Models

Young-Laplace

General specifications

Sample dimensions

Maximum sample space

∞ × ∞ × ∞ (W × D × H)

Instrument dimensions

Footprint

84 mm × 32 mm (W × D)

Height

112 mm

Weight (without accessories)

0.85 kg

Environment

Operating temperature

10 °C to 40 °C

Humidity

without condensation

Interfaces

PC

USB 3.0

Housing and peripherals

Compartment

aluminum

Power supply

Voltage

5 V (powered via USB)

Power consumption

4.5 W

Produkte vergleichen